CML stainless steel tube fittings in SS304, SS316L and Duplex 2205

Materials

CML tube fittings are listed in SS316L, SS304 and Duplex 2205. Composition limits below are from ASTM A479.

SS316L

UNS S31603 / EN 1.4404

Code S6. Austenitic grade with 2–3 % molybdenum and low carbon. Typically chosen where chlorides or process chemicals are present.

SS304

UNS S30400 / EN 1.4301

Code S4. Austenitic chromium-nickel grade without molybdenum. Typically chosen for general-purpose service in milder environments.

Duplex 2205

UNS S32205 / S31803, EN 1.4462

Code DP. Austenitic-ferritic grade with higher chromium, molybdenum and nitrogen. Typically chosen where higher strength or resistance to chloride stress corrosion cracking is needed.

Chemical composition

Limits in percent by weight, maximum unless a range is shown, from ASTM A479/A479M (ASME SA-479, 2023 edition), Table 1. Iron is the balance. EN numbers are the corresponding EN 10088 designations.

GradeUNSENCMnPSSiCrNiMoN
SS316LS316031.44040.0302.000.0450.0301.0016.0–18.010.0–14.02.00–3.00–
SS304S304001.43010.082.000.0450.0301.0018.0–20.08.0–10.5––
Duplex 2205S322051.44620.0302.000.0300.0201.0022.0–23.04.5–6.53.0–3.50.14–0.20
Duplex 2205S318031.44620.0302.000.0300.0201.0021.0–23.04.5–6.52.5–3.50.08–0.20

Minimum mechanical properties

Annealed condition, ASTM A479/A479M Table 2.

GradeUNSTensile strength, min. MPaYield strength, min. MPa
SS316LS31603485170
SS304S30400515205
Duplex 2205S32205655450
Duplex 2205S31803620450

These are standard limits for the grade, not test results for a specific lot. Pressure availability depends on tube O.D. and is listed on the Technical page. Material choice for a given medium and temperature remains the responsibility of the system designer.

Documentation

Material test certificates (MTC) available on request. Ask us about material documentation with your inquiry. State the grade and any standard you need it to reference.

Request a quote Applications